A quick and effective method of cleaning objects prior to plating. The cleaning process uses an electrolytic bath, similar to plating operations. The 2 lb. size makes 8 gallons - 5 lb. size makes 20 gallons. Use with a stainless steel anode. Clean with the solution heated from 120° to 160° F (50° to 71° C) at 2 to 6 volts for 15 to 30 seconds.
3-5 business days
Buyers are responsible for any customs and import taxes that may apply. I'm not responsible for delays due to customs.
But please contact me if you have any problems with your order.
We Ship by First Class Mail USPS for USA orders. For international orders we ship Fed Ex.